Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.77 g/cc | 0.281 lb/in³ | |
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
Density | 7.77 g/cc | 0.281 lb/in³ | |
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |