Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.73 g/cc | 0.279 lb/in³ | |
Williams Advanced Alloys WS217 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum AL 4466™ Ferritic Stainless Steel Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:outstanding resistance to chloride pitting and crevice corrosion, improved resistance over austenitic stainless steels to ch.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Annealed Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 316°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 427°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |