Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.69 g/cc | 0.278 lb/in³ | Sintered |
Kinetics MIM 440C Stainless Steel Martensitic stainless steel. Excellent strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Often used for automotive, cutlery, industrial equipment, power han.. |