Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.52 g/cc | 0.272 lb/in³ | Sintered |
Kinetics MIM K1 Kinetics Custom Alloy K1 is a custom alloy that provides very high wear resistance. Possible applications include agricultural implements, high security lock components, and wear surface applications in assemblies. This .. |