Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.355 g/cc | 0.2657 lb/in³ | |
Lucas-Milhaupt Clean & Bright & Brite Tin/ Silver Solder Characteristics:This alloy is considered to be high strength solders. It has much higher creep strengths than the tin/lead solders. It is a good color match for stainless steel, and used with the p.. |