Physical Properties Metric English Comments
Density 7.353 g/cc
0.2656 lb/in³
American Elements Samarium Nanoparticles
General DescriptionSamarium (Sm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Samarium Particles are typically 10 - 50 nanometers (nm) with specif..