Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.34 g/cc | 0.265 lb/in³ | |
Indium Corp. Indalloy 123 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.34 g/cc | 0.265 lb/in³ | |
Williams Advanced Alloys WS226A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.34 g/cc | 0.265 lb/in³ | |
ATI Allegheny Ludlum ALFA-II™ Stainless Steel Type 406 Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat.. |