Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.700 g/cc | 0.2059 lb/in³ | |
Reade Advanced Materials Calcia Stabilized Zirconium Oxide (ZrO2 + CaO) Description: Produced by thermal processes. Used in wear parts, engine and machine components, mill media, refractories, ceramic pigments. fuel cells, laser, and capacitors.Forms Available: Various.. |
|||
Density | 5.700 g/cc | 0.2059 lb/in³ | |
Reade Advanced Materials Zirconium Oxide, Hafnia Stabilized (ZrO2 + HfO2) Description: A fused high density monoclinic grain. Used in fluid beds as loose insulation, setting grain and as a source of zirconium.Forms Available: Available in both USS mesh and F sizesInforma.. |