Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.95 g/cc | 0.179 lb/in³ | |
Anderman Ceramics EREY99 Yttrium Oxide Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |