Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.75 g/cc | 0.172 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0475 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 4.75 g/cc | 0.172 lb/in³ | |
Ferro EG 2964 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins.. |