Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.28 g/cc | 0.155 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Density | 4.28 g/cc | 0.155 lb/in³ | |
Schott SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.28 g/cc | 0.155 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Density | 4.28 g/cc | 0.155 lb/in³ | |
Schott N-LAF21 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.28 g/cc | 0.155 lb/in³ | |
Corning 8870 Potash Lead Crushed Glass Used for sealing and other applications.Information provided by Corning Incorporated. |