Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.42 g/cc | 0.124 lb/in³ | ASTM C20 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |