Polymer Property : Density = 3.36 g/cc
Polymer Property :
Density =
3.36 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
3.36
g/cc
0.121
lb/in³
Ceradyne Ceralloy® 7712 Al2O3-SiC
Applications:slot mode absorbersInformation provided by Ceradyne Company