Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.11 g/cc | 0.112 lb/in³ | |
Schott N-BALF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.11 g/cc | 0.112 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 3.11 g/cc | 0.112 lb/in³ | DIN EN 623-2 |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |