Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.40 - 3.10 g/cc | 0.0506 - 0.112 lb/in³ | Average value: 2.24 g/cc Grade Count:75 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |