Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.07 g/cc | 0.111 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Density | 3.07 g/cc | 0.111 lb/in³ | DIN EN 623-2 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |