Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.165 g/cc | 0.07822 lb/in³ | ASTM D4894 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |
|||
Density | 2.165 g/cc | 0.07822 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® A.20 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |