Density 2.115 g/cc
0.07641 lb/in³
Pyrotek Pyrocast 220HT Refractory Castable
Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r..