Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.071 g/cc | 0.07482 lb/in³ | |
Materion AlBeMet® AM 162 HIP'd Billet, Annealed This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) .. |
|||
Density | 2.071 g/cc | 0.07482 lb/in³ | |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Density | 2.071 g/cc | 0.07482 lb/in³ | |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |