Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.0142 g/cc | 0.072760 lb/in³ | |
Saint-Gobain Chemfab® 6 Primary PTFE-Coated Glass Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: .. |