Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 19.7 g/cc | 0.712 lb/in³ | |
Goodfellow Tungsten 75/Rhenium 25 Alloy When used with Tungsten the alloy is an important high temperature thermocouple wire. The alloy can also be used as a filament.Information provided by Goodfellow. |