Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 18.3 g/cc | 0.661 lb/in³ | |
MarkeTech 96-3-1 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Density | 18.3 - 18.7 g/cc | 0.661 - 0.676 lb/in³ | |
H.C. Starck HPM 1850W Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Density | 18.3 - 18.7 g/cc | 0.661 - 0.676 lb/in³ | |
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |