Physical Properties Metric English Comments
Density 18.2 g/cc
0.658 lb/in³
Wieland BioPortadur Casting Alloy
Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental