Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 18.1 g/cc | 0.654 lb/in³ | |
MarkeTech 95-3-2 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |