Physical Properties Metric English Comments
Density 18.0 g/cc
0.650 lb/in³
Hogen HM3000 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l..
Density 18.0 g/cc
0.650 lb/in³
Hogen HM3050 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
Density 18.0 g/cc
0.650 lb/in³
Mi-Tech Metals HD18 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm..
Density 18.0 g/cc
0.650 lb/in³
Mi-Tech Metals HD18D Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..
Density 18.0 g/cc
0.650 lb/in³
Wieland Porta P6 PFM Alloy
Gold-platinum-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental
Density 18.0 g/cc
0.650 lb/in³
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
Density 18.0 g/cc
0.650 lb/in³
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.