Polymer Property : Density = 17.4 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 17.4 - 17.8 g/cc
0.629 - 0.643 lb/in³
H.C. Starck HPM 1760 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Density 17.4 - 17.8 g/cc
0.629 - 0.643 lb/in³
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet
Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo..
Density 17.4 g/cc
0.629 lb/in³
CMW® ELKONITE 2088 very high refractory, tungsten, silver
ELKONITE® 2088 has a very high refractory content and is not considered in the normal family of make and break contacts. It is used in special applications where weight or hardness together with co..
Density 17.4 g/cc
0.629 lb/in³
CMW® ELKONITE® 2188 Infiltrated Tungsten Silver Contact Material
High wear resistance and reliability.Information provided by CMW Inc.