Polymer Property : Density = 17.3 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 17.3 - 17.7 g/cc
0.625 - 0.639 lb/in³
H.C. Starck HPM 1750 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Density 17.3 - 17.7 g/cc
0.625 - 0.639 lb/in³
H.C. Starck HPM 1751 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Density 17.3 g/cc
0.625 lb/in³
CMW® ELKONIUM 76 gold based alloy
Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to ..