Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 15.3 - 15.9 g/cc | 0.553 - 0.574 lb/in³ | |
H.C. Starck WCu 80/20 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |