Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 15.1 g/cc | >= 0.546 lb/in³ | |
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite RWMA Class 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is .. |
|||
Density | >= 15.1 g/cc | >= 0.546 lb/in³ | |
Hogen H20S, 26 Silver/74 Tungsten PM Metal Composite RWMA Class EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica.. |
|||
Density | >= 15.1 g/cc | >= 0.546 lb/in³ | |
Mi-Tech Metals CW80 80 Tungsten/20 Copper PM Metal Composite RWMA Class 12.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is specifi.. |
|||
Density | >= 15.1 g/cc | >= 0.546 lb/in³ | |
Mi-Tech Metals SW74 26 Silver/74 Tungsten PM Metal Composite RWMA Class EDMMi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica.. |
|||
Density | 15.1 g/cc | 0.546 lb/in³ | |
Wieland 1605 Wilaform Gold Red gold for all kinds of decoration manufacturing.Applications: casting, laminar decoration, pipes, tubingDental |