Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 15.0 g/cc | 0.542 lb/in³ | |
Momentive Performance Materials Tantalum Carbide (TaC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Density | 15.0 g/cc | 0.542 lb/in³ | |
Wieland Porta SMK 82 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Density | 15.0 - 15.3 g/cc | 0.542 - 0.553 lb/in³ | |
China Tungsten YG3X Tungsten Carbide for Dies and Wear Part Making For drawing of steel non-ferrous metal and alloy wire of |