Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.77 g/cc | 0.5336 lb/in³ | |
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated For arcing and current carrying electrical contacts; household and power circuit breakers.Information provided by CMW Inc. |
|||
Density | 14.77 g/cc | 0.5336 lb/in³ | |
Cadi 35WS Tungsten Silver Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |