Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.72 g/cc | 0.5318 lb/in³ | |
Williams Advanced Alloys WS487 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |