Polymer Property : Density = 14.65 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.65 - 14.85 g/cc
0.5293 - 0.5365 lb/in³
China Tungsten Z20 Tungsten Carbide for Mining Purposes
Excellent wear resistance and toughness, for pillar bit drills.Information provided by China Tungsten