Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.51 g/cc | 0.5242 lb/in³ | |
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 14.51 g/cc | 0.5242 lb/in³ | |
Williams Advanced Alloys WS280B Solder (Au80/Sn20) All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |