Density 13.83 g/cc
0.4996 lb/in³
CMW® ELKONITE® 3W3 Tungsten Copper material ASTM B702
For arcing and current carrying electrical contacts, power transformer contacts, resistance welding electrodes.Information provided by CMW Inc.