Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.6 - 13.8 g/cc | 0.491 - 0.499 lb/in³ | |
China Tungsten ZY31 Tungsten Carbide for Mining Purposes High impact toughness, for hi-speed wire mills for primary and intermediate rolling of mild wire rods.Information provided by China Tungsten |