Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 12.65 g/cc
0.4570 lb/in³
CMW® ELKONITE® TC20 Tungsten Carbide Copper material
For electroforging and electrical upsetting dies.Information provided by CMW Inc.