Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.36 g/cc | 0.4465 lb/in³ | |
Wall Colmonoy COLMONOY® 730 - Nickel-Chromium-Tungsten Matrix Alloy Description and Application: A tough nickel-chromium-boron matrix alloy holds extremely hard tungsten-carbide particles. Finer mesh tungsten carbide than Colmonoy 750. Used on pump plungers and sl.. |