Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.1 g/cc | 0.365 lb/in³ | |
CMW® ELKONIUM 18 silver, copper, cadmium alloy The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability.. |
|||
Density | 10.1 g/cc | 0.365 lb/in³ | |
CMW® ELKONIUM 22 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |