Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.921 g/cc | 0.06939 lb/in³ | Slurry |
Omya OMYACARB® UF - FL Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water.. |
|||
Density | 1.921 g/cc | 0.06939 lb/in³ | Slurry |
Omya OMYAFLOW® UF - SY Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Decorative paints.Information supplied by Omya North America. |