Physical Properties Metric English Comments
Density 1.9134 g/cc
0.069120 lb/in³
Saint-Gobain Chemfab® 3 Tear Resistant PTFE-Coated Glass
Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas..
Density 1.9134 g/cc
0.069120 lb/in³
Saint-Gobain Chemfab® 6 Anti-Static PTFE-Coated Glass
Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electri..