Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.645 g/cc | 0.05943 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |