Polymer Property : Density = 1.559 g/cc
Polymer Property :
Density =
1.559 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.559
g/cc
0.05632
lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT
LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber.