Polymer Property : Density = 1.556 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.556 g/cc
0.05621 lb/in³
ISO 1183
Tisan TISAPET® 30% Glass Reinforced Polyethylene Terephthalate
Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a..