Polymer Property : Density = 1.552 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.552 g/cc
0.05607 lb/in³
ISO 1183
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds