Polymer Property : Density = 1.540 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.540 g/cc
0.05564 lb/in³
Saint-Gobain Chemfab® q-GUARD® 215 Insulation Jacketing
Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fibergl..