Polymer Property : Density = 1.493 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.493 g/cc
0.05394 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® CE15315 BK010 PBT  (Unverified Data**)
Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..