Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.473 g/cc | 0.05322 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Density | 1.473 g/cc | 0.05322 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal (Asia Pacific) LNP STAT-KON* KEP33 is a compound based on Acetal resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Density | 1.473 g/cc | 0.05322 lb/in³ | ISO 1183 |
Stir SpA SR 80 2 (PVC) Application: Primary type TI 1Information provided by STIR SpA |