Polymer Property : Density = 1.408 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.408 g/cc
0.05087 lb/in³
ISO 1183
Stir SpA SPI 78 ATC (PVC)
Application: Ecological PlugsInformation provided by STIR SpA