Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.407 g/cc
0.05083 lb/in³
JIS-Z-8807
Denka VINYKON S3097 PVC, S grade for refrigerator gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..